极地低温下高强钢对接焊缝连接力学性能
|
|
曹换, 蔡骜, 谌扬宇, 左文康, 陈满泰
|
Behavior of High Strength Steel Butt Joints at Arctic Low Temperatures
|
|
CAO Huan, CAI Ao, CHEN Yangyu, ZUO Wenkang, CHEN Mantai
|
|
表3 常温和低温环境下高强钢对接焊缝拉伸试件力学性能指标
|
Tab.3 Mechanical properties of high strength steel butt joint tensile specimens at ambient and low temperatures
|
|
| 试件 | σ0.2/MPa | σu/MPa | εf/% | | | | | | | | | | | H8W0T25 | 653.6 | 764.6 | 10.6 | 1.04 | 1.09 | 0.55 | 0.91 | 0.97 | 0.46 | 1.00 | 1.00 | 1.00 | | H8W0T25R | 655.8 | 765.3 | 12.4 | 1.05 | 1.09 | 0.64 | 0.92 | 0.97 | 0.54 | 1.00 | 1.00 | 1.00 | | H8W0T-20 | 662.2 | 799.8 | 16.5 | 0.97 | 1.00 | 0.67 | 0.91 | 0.94 | 0.69 | 1.01 | 1.05 | 1.43 | | H8W0T-40 | 661.8 | 815.2 | 18.1 | 1.02 | 1.09 | 0.76 | 0.90 | 0.95 | 0.70 | 1.01 | 1.07 | 1.57 | | H8W0T-60 | 664.9 | 836.7 | 19.3 | 1.00 | 1.06 | 0.80 | 0.90 | 0.96 | 0.69 | 1.02 | 1.09 | 1.68 | | H8W0T-75 | 678.8 | 861.9 | 16.9 | 0.93 | 1.00 | 0.66 | 0.91 | 0.96 | 0.70 | 1.04 | 1.13 | 1.47 | | H8W2T25 | 708.0 | 788.0 | 21.1 | 1.13 | 1.12 | 1.09 | 0.86 | 0.82 | 1.20 | 1.00 | 1.00 | 1.00 | | H8W2T25R | 704.2 | 786.5 | 19.8 | 1.12 | 1.12 | 1.02 | 0.86 | 0.81 | 1.13 | 1.00 | 1.00 | 1.00 | | H8W2T-20 | 699.9 | 775.1 | 17.9 | 1.02 | 0.97 | 0.72 | 0.84 | 0.77 | 0.97 | 0.99 | 0.98 | 0.88 | | H8W2T-40 | 706.6 | 801.8 | 21.2 | 1.09 | 1.08 | 0.89 | 0.85 | 0.77 | 1.18 | 1.00 | 1.02 | 1.04 | | H8W2T-60 | 726.3 | 858.8 | 21.0 | 1.10 | 1.09 | 0.87 | 0.84 | 0.81 | 1.15 | 1.03 | 1.09 | 1.03 | | H8W2T-75 | 741.5 | 873.0 | 22.4 | 1.02 | 1.01 | 0.88 | 0.86 | 0.81 | 1.24 | 1.05 | 1.11 | 1.10 |
|
|
|